Usually you use fuming nitric acid with or without sulfuric acid depending if you have copper bondings.

https://www.semitracks.com/reference-material/failure-and-yi...



In my experience just hot sulfuric acid works fairly well if you're looking to just get the die out. Just don't leave it too long or you won't have any bond pads left...